What are dispersants?
Dispersants are chemical additives that promote the uniform distribution and stability of pigments and mineral fillers in various formulations, including water-based paints, paints, colorants, and ceramic systems. In water-based paints, they stabilize pigments and mineral fillers in an aqueous suspension, preventing flocculation and sedimentation. The most commonly used is sodium polyacrylate, which acts on the surface of the particles, creating repulsion between them. Typical dosage: 0.2–0.5% by total weight.
For micronized pigments , the choice of dispersant affects wetting, tinting strength, and suspension stability. To achieve the correct viscosity and rheology, dispersants work synergistically with cellulose ethers such as HEC and HPMC.
In short
- Typical dosage: 0.2–0.5% of the total weight of the formulation
- Mechanism: electrostatic stabilization
- Add to the aqueous phase before the pigments
- Compatible with iron oxides, TiO₂, calcium carbonate, kaolin
- Stable from pH 7 to pH 10
How sodium polyacrylate works
Sodium polyacrylate is a water-soluble anionic polymer. In aqueous solution, the carboxylate groups (–COO⁻) dissociate and impart a negative charge to the polymer chain. When the polyacrylate is added before the pigments, the chains adsorb onto the surface of the pigment and filler particles, giving them a uniform negative charge. The so-charged particles repel each other electrostatically, remaining in a stable suspension. Among inorganic dispersants, sodium hexametaphosphate (SHMP) is also used as a sequestrant and dispersant in ceramics, colorants, and water treatment.
Technical properties
| Parameter | Value |
|---|---|
| Stabilization mechanism | Electrostatic (anionic) |
| Typical dosage in water-based paints | 0.2–0.5% by total weight |
| pH stability | pH 7–10 (optimal pH 8–9) |
| Compatibility with surfactants | Good with anionics and non-ionics; avoid cationics |
| Sensitivity to electrolytes | Moderate: avoid excess divalent salts (Ca²⁺, Mg²⁺) |
| Effect on viscosity | Reduces grinding viscosity, slightly increases final viscosity |
Dosages for pigment and filler
| Pigment / Filler | Polyacrylate dosage | Notes |
|---|---|---|
| Calcium carbonate (CaCO₃) | 0.2–0.3% | Low specific surface area, low dosage is sufficient |
| Kaolin | 0.2–0.4% | Good compatibility, rapid dispersion |
| TiO₂ | 0.3–0.5% | High specific surface area, higher dosage |
| Iron oxides (red, yellow, black) | 0.3–0.5% | Excellent compatibility, no color alteration |
| Talc | 0.2–0.3% | Platelet filler, easy dispersion |
Order of addition in the formulation
- Add the polyacrylate to the water under slow agitation before any other component.
- Add the other water-soluble additives (wetting agent, defoamer, jar biocidal, HEC).
- Add the pigments and fillers under high-speed agitation (dissolving).
- Complete the grinding to the desired fineness (typically <20 μm for wall paints).
- Add the acrylic binder and other components during the completion phase.
Common errors to avoid
- Adding after the pigments: the polyacrylate cannot disperse correctly on already aggregated particles
- Overdosing: excess free polyacrylate in solution can increase the water sensitivity of the dried film
- Using with cationic surfactants: precipitation due to ionic incompatibility
- Formulating at an acidic pH: below pH 7, the carboxylate groups become protonated and the polyacrylate loses effectiveness
FAQ — Frequently Asked Questions about Dispersants for Water-Based Paints
What is the correct dosage of sodium polyacrylate in water-based paints?
0.2–0.5% by total weight of the formulation. The exact dosage depends on the specific surface area of the pigment: TiO₂ and iron oxides require 0.3–0.5%; fillers such as calcium carbonate and talc require 0.2–0.3%.
When is the polyacrylate added to the formulation?
Always in the initial aqueous phase, before adding the pigments and fillers. This ensures maximum dispersion efficiency during grinding.
Is sodium polyacrylate compatible with iron oxides?
Yes, it is fully compatible with red, yellow, black, and brown iron oxides, without altering their color or dispersion.
What happens if too much polyacrylate is used?
Overdosing leaves free polyacrylate in solution, which can increase the water sensitivity of the dried film and reduce wash resistance. Follow the recommended dosage.
Is sodium polyacrylate compatible with HEC?
Yes, it is fully compatible with HEC (hydroxyethyl cellulose) and HEURs. Both are added to the initial aqueous phase without interfering with each other.
What is the difference between a dispersant and a wetting agent in water-based paints?
The wetting agent lowers the surface tension of the water to facilitate the initial wetting of the pigment particles. The dispersant stabilizes the wetted particles, preventing them from re-aggregating (flocculation). Both are used in formulation: first the wetting agent, then the pigments are kept in a stable suspension by the dispersant.
Can non-ionic dispersants be used in water-based paints?
Yes, non-ionic dispersants work through a steric mechanism rather than an electrostatic one and are useful in formulations with variable pH or cationic surfactants. Their cost is generally higher, and their effectiveness on inorganic pigments is lower than that of polyacrylates.
How do you choose the right dispersant for a wall paint?
For water-based wall paints, 40% sodium polyacrylate is the standard choice: dosage of 0.3–0.5% for TiO₂ and iron oxides, formulation pH of 8–9, compatible with HEC and acrylic binders.